Photoresists & Manufacturers

Below is a list of photoresist manufacturers and a table of photoresists. We do not claim that either of these is comprehensive. There are other manufacturers and photoresists, but these are some of the more common ones. Some of the names given in the photoresist table are the names of series and not individual resists. A series may include many individual photoresists. Some photoresists have more information than others. We only included information that was easily and quickly obtainable from the manufacturers' websites. Many of them may have more uses or applications than noted here. Some manufacturers provide datasheets or product guides and the links for those have been included in the table. If you desire more information about a specific photoresist please check the manufacturer's website or contact the manufacturer.



AZ Electronic Materials Dow DuPont
Electra Polymers Ltd. Eternal Chemical Fujifilm Electronic Materials
Hitachi Chemical HiTech Photopolymere AG JSR Micro
Kolon Industries MacDermid MicroChem
Rohm and Haas (subsidiary of Dow) Sumitomo Chemical Tokyo Ohka Kogyo Co., Ltd.





Manufacturer Photoresist Tone Thickness
(in µm)
Wavelengths (in nm)
Aspect Ratio/
Primary Uses/Applications
AZ AX series     193   contact holes, line/space
AZ DX and EXP series     248   multi-purpose, back end
AZ HiR 1075 Positive 0.6-1.2 i Ultra high line/space, contact holes
AZ MiR 701 Positive 0.6-3.0 i High line/space, contact holes
AZ MiR 703 Positive 0.8-1.4 i Mid-range line/space, contact holes
AZ MiR 900 Positive 2-4.5 i High aspect ratio line/space
AZ N6000 Negative 0.6-10 i   ion implant, high speed
AZ nLOF 2000 Negative 1.5-10 i   lift off
AZ nLOF 5000 Negative 0.75-1.5 i High lift off
AZ 3300 Positive 1-2.5 ghi   general purpose
AZ 3300-F Positive 0.8-5 ghi   general purpose, high speed
AZ 1500 Positive 0.4-4 ghi   general purpose, wet etch
AZ N4000 Negative 2.5-5.5 gh    
AZ P4000 series Positive 2-55 gh 2:1  
AZ 4500 series Positive 2-55 gh 2:1  
AZ 9200 series Positive 3-50 ghi 3:1  
AZ 10XT Positive 4-50 ghi 3:1 plating and etch applications
AZ 50XT Positive 15-65 gh 3:1 plating and etch applications
AZ PLP-30   6-25 gh 2:1  
AZ PLP-40   20-30 gh 2:1  
AZ 5XT series Positive 3-5 ghi 2:1  
AZ 12XT series Positive 5-20 ghi 4:1 Cu RDL and TSV applications
AZ 40XT series Positive 20-100 ghi 4:1 etch and plating applications
AZ 125nXT series Negative 20-120 ghi 6:1  
AZ 5nXT/15nXT Negative 5-20 ghi 3:1 Cu RDL and TSV plating/etch
AZ TX 1311   3-5 DUV 15:1  
DOW Laminar series         dry film photoresists for alkaline and acid etch and pattern plating
DOW Eagle 2100 ED Negative       printed circuit board manufacturing
DOW Photoposit series         roller coated photoresists for printed circuit boards
DOW Epic 2135     193   65 nm and 90 nm node processes
DOW UVN 2300 Negative   DUV   implant and cell open applications
DOW UV series Positive 0.5-3 248    
DOW MCPR i7010N Positive >0.35 i   general purpose
DOW Megaposit SPR 955-CM Positive >0.35 i   general purpose
DuPont Riston Etchmaster 213/830 Negative 30 350-380   dry film resist, acid etch, chemical milling
DuPont Riston Goldmaster GM100   50/75/100 350-380   dry film resist, gold plating, adhesion to various metals
DuPont Riston MultiMaster MM100i/MM500   30/40/50/65/75 350-380   dry film resist, general purpose, alkaline etch, gold plating
DuPont Riston PlateMaster PM200/PM300 Negative 38/40/50/75/100 350-380   dry film resist for copper, tin, tin/lead plating
DuPont Riston TentMaster TM200i Negative 30/38 350-380   dry film resist, tent and etch processes, acid etch
DuPont Riston Laser LDI 300/500/7000/7200/8000 Negative 30/38/40/50/62/75 355/405   dry film resist, laser direct imaging
DuPont Riston FX 250/500/900 Negative 15,30,40,50,62 350-380   dry film resist, Ni/Au plating, fine lines, chemical milling, acid etch
Eternal Etertec Series   12-50     dry film resists, plating, print-and-etch, tent-and-etch, chemical milling, PKG
Eternal Laminar Series   24-101     dry film resists, plating, print-and-etch, tent-and-etch, LDI for some
Fujifilm FEP-100 Positive   e-beam   e-beam direct write
Fujifilm FEN-100 Negative   e-beam   e-beam direct write
Fujifilm GAR series     193   various
Fujifilm GKR series     248   various
Fujifilm SC series Negative >1 g   general purpose, resistant to common silicon etchants
Fujifilm HNR series Negative >1 g    
Fujifilm HR series Negative >1 g    
Fujifilm IC series Negative >1 g    
Fujifilm HPR 500 series Positive >0.75 g   ion implant, wet and dry etching
Fujifilm OCG 825   >0.75 g    
Fujifilm HiPR 6500 series   >0.75 gi    
Fujifilm OiR series Positive >0.25 gi   various
Fujifilm FHi series   >0.25 gi    
Fujifilm GiR 1102   0.25-0.4 i    
Fujifilm PMMA Positive   DUV/e-beam 7:1 various
Hitachi RD series   10/15/20/25 355-405 High dry film, DLP and UV-LDI systems
Hitachi DL series   29/32/38   High dry film, DLP systems
Hitachi SL series   29/33/38   High dry film, UV-LDI systems
Hitachi RY series   25   High dry film, PKG
Hitachi H series   25/30/34/38/45   High dry film, PCB production, tenting
Hitachi HM series   56/75/112   High dry film, electro-forming
Hitachi FR series   25/38/50     dry film, FPC production
Hitachi FZ series   20/25/30/35     dry film, solder resist, PKG
HiTech DiaEtch 101 Negative   300-350   Dip-coating application for various metallic substrates
HiTech DiaEtch 102 Negative >25 300-450   Dip-coating application for printed circuit boards
HiTech DiaEtch 120 Negative >25 300-450   Roller-coating application for printed circuit boards
HiTech DiaEtch 122 Negative >25 300-450   Roller-coating application for various metallic substrates
HiTech DiaPlate   5-500     Electroforming process, adhesion to various substrates
JSR Micro ARX series Positive   ArF(193)   line/space, contact hole, implant
JSR Micro M series Positive   KrF(248)   line/space, contact hole, implant
JSR Micro V series Positive   KrF(248)   implant
JSR Micro NDS series Negative   KrF(248)   implant
Kolon Trumask Negative       inner layer, lead frames, BGA, roller or dip-coated
MacDermid PMGI and LOR Positive <0.05 - >8 DUV/240-290   Sacrificial Layer, Bi-layer Lift-off
Microchem SU-8 series Negative <1 - >300 Near UV/350-400 10:1 Permanent applications
Microchem KMPR 1000 Negative <4 - >120 i High MEMS, electrolytic plating, DRIE applications
Microchem PMMA Positive <0.1 - >5 DUV/e-beam/x-ray High T-gates, e-beam and x-ray processes, protective coatings, sacrificial layer
Sumitomo Sumiresist Positive        